| Sign In | Join Free | My wneducation.com |
|
Brand Name : JINHAIHU
Model Number : DSC-600
Certification : ISO 9001
Place of Origin : BEIJING, CHINA
MOQ : 1 set
Payment Terms : T/T,L/C,Western Union,MoneyGram,D/A,D/P
Supply Ability : 20 sets per month
Delivery Time : 7-15 working days
Packaging Details : Conventional export wooden crates
Product name : Plastics-Differential scanning calorimeter(DSC)
Model : DSC-600
Certificate : ISO, CE
DSC Range : 0~±500mW
Temperature Range : Room temperature ~ 800℃ Air cooling
Heating Rate : 0.1~80 ℃/min
Temperature Resolution : 0.1℃
Temperature Fluctuation : ±0.1℃
Plastics-Differential scanning calorimeter(DSC)
Brief introduction of the instrument:
Differential scanning calorimetry (DSC) is a classic thermal analysis technique for measuring thermal effects under programmed temperature control. It is widely applied in multiple material and chemical fields, including R&D, process optimization, quality control, and failure analysis. Using DSC, one can study phase transitions in inorganic materials, melting and crystallization processes of polymer materials, drug polymorphism, and solid/liquid phase ratios in oils and fats.
Instrument use:
Measurements include physical and chemical changes related to heat, such as glass transition temperature, melting point, melting temperature, crystallization and crystallization heat, phase transformation reaction heat, thermal stability, curing/crosslinking, and oxidation induction period of the product.
Reference standard:
Technical parameter:
| DSC | DSC-600 Differential Scanning Calorimeter |
| DSC Range | 0~±500mW |
| Temperature Range | Room temperature ~ 800℃ Air cooling |
| Heating Rate | 0.1~80 ℃/min |
| Temperature Resolution | 0.1℃ |
| Temperature Fluctuation | ±0.1℃ |
| Temperature Repeatability | ±0.1℃ |
| DSC Noise | 0.01mW |
| DSC Resolution | 0.01mW |
| DSC Accuracy | 0.01mW |
| DSC Sensitivity | 0.01mW |
| Temperature Control Mode | Heating, constant temperature (full program automatic control) |
| Curves Scan | Heating scan |
| Atmosphere Control | Instrument automatically switches |
| Display | 24bit color 7-inch LCD touch-screen display |
| Data Interface | Standard USB interface |
| Parameter Standards | With a standard substance; a key calibration function; the user can correct the temperature and enthalpy personally. |
| Remark | All the technical indicators can be adjusted according to user needs. |





|
|
Plastics 500mW Differential Scanning Calorimeter Instrument DSC-600 Images |